中文名304不锈钢/06Cr19Ni10外文名304 stainless steel/SUS304特 点耐腐蚀,韧性好半成品状态热轧板,冷拔管磁 性无磁性国 标GB/T 3280-2015
物理性能
304
|
C
|
Mn
|
P
|
S
|
Si
|
Cr
|
Ni
|
要求,%
|
≤0.08
|
≤2.00
|
≤0.045
|
≤0.030
|
≤1.00
|
18.0–20.0
|
8.0-11.0
|
304
|
C
|
Mn
|
P
|
S
|
Si
|
Cr
|
Ni
|
N
|
要求,%
|
≤0.07
|
≤2.00
|
≤0.045
|
≤0.030
|
≤0.75
|
17.5–19.5
|
8.0–10.5
|
≤0.10
|
SUS 304
|
C
|
Mn
|
P
|
S
|
Si
|
Cr
|
Ni
|
要求,%
|
≤0.08
|
≤2.00
|
≤0.045
|
≤0.030
|
≤1.00
|
18.0–20.0
|
8.0-10.5
|
SUS 304
|
C
|
Mn
|
P
|
S
|
Si
|
Cr
|
Ni
|
要求,%
|
≤0.08
|
≤2.00
|
≤0.045
|
≤0.030
|
≤1.00
|
18.0–20.0
|
8.0-10.5
|